I bought these heated gloves on Amazon and been happy with them so far. On low, which keep my hands comfortably warm, they run for a little over 5 hours before shutting itself off. How long should I run these before I charge the batteries? When I do charge the batteries, should I let the charger run till the red LED on the charger turn green indicating a full charge, or should I stop charging at 80% to prolong battery life? I can take voltage measurements to determine state of charge of the batteries.
I have one data point so far:
Full charge = 8.4 V
Run for 4 hours on low = 7.14 V or 3.57 V per cell
I will run them till they shut off and take another voltage measurement to see if LVC is set to a safe level (which I believe is 3.2 V for LiPo ?).


I have one data point so far:
Full charge = 8.4 V
Run for 4 hours on low = 7.14 V or 3.57 V per cell
I will run them till they shut off and take another voltage measurement to see if LVC is set to a safe level (which I believe is 3.2 V for LiPo ?).