mrmojorising
Established
I came across a Fiido for cheap and had no ongoing projects, so I thought why not. I wanted a project to test out a battery using 46950 cells, and this setup was perfect.
Specs:
Fiido Q1S Frame
2x Stock Q1S geared hub motors, front & rear
20S1P EVE G16 4695E Battery (72V 32Ah, 120A max discharge). JNFN (ANT) BMS
Monorim dual crown air forks
Flipsky FT85BD dual motor controller
Brake lights, horn, and headlights using the Flipsky's dedicated 12V outputs
Custom 3D printed controller housing (Black ABS)
The two stock motors provide great torque at 72V, but max out at about 50kph due to gear limitation. They easily handle being fed 20amps each with 5amps of Flux weakening (which really only adds a few kph at most). All in all, a super fun little scooter at this power
A few notes on the battery as this is definitely not a common, nor recommended way of using these cells. They were spot-welded using Al-Ni composite strips on the postitive terminal (which is Aluminium). These strips help facilitate enough heat to produce a decently solid weld, which can then be welded on top of with a Cu-SS sandwich. This really pushed the limits of my Awithz P30C welder, but I was happy with the result. The Cu is 0.2mm x 20mm with 0.1mm SS on top.



Specs:
Fiido Q1S Frame
2x Stock Q1S geared hub motors, front & rear
20S1P EVE G16 4695E Battery (72V 32Ah, 120A max discharge). JNFN (ANT) BMS
Monorim dual crown air forks
Flipsky FT85BD dual motor controller
Brake lights, horn, and headlights using the Flipsky's dedicated 12V outputs
Custom 3D printed controller housing (Black ABS)
The two stock motors provide great torque at 72V, but max out at about 50kph due to gear limitation. They easily handle being fed 20amps each with 5amps of Flux weakening (which really only adds a few kph at most). All in all, a super fun little scooter at this power
A few notes on the battery as this is definitely not a common, nor recommended way of using these cells. They were spot-welded using Al-Ni composite strips on the postitive terminal (which is Aluminium). These strips help facilitate enough heat to produce a decently solid weld, which can then be welded on top of with a Cu-SS sandwich. This really pushed the limits of my Awithz P30C welder, but I was happy with the result. The Cu is 0.2mm x 20mm with 0.1mm SS on top.



Attachments
-
IMG_20260216_152119.jpg3 MB · Views: 17 -
Screenshot_2026-02-16-19-22-10-21_425154530a3df2b6520d5742e232d9aa.jpg527.6 KB · Views: 16 -
Screenshot_2026-02-16-19-22-06-35_425154530a3df2b6520d5742e232d9aa.jpg503.5 KB · Views: 11 -
Messenger_creation_DC2EE7D7-9434-4731-B23B-BC3F48A63107.jpg157.1 KB · Views: 16 -
IMG_20260306_132501.jpg2.6 MB · Views: 16 -
IMG_20260225_215036.jpg1.8 MB · Views: 15 -
IMG_20260225_215024.jpg2.3 MB · Views: 14 -
IMG_20260217_145105.jpg2.7 MB · Views: 14 -
IMG_20260217_142906.jpg2.5 MB · Views: 17
Last edited: