Hi,
So I had battery problems and decided to get a new BMS. I'm happy that everything went well and have the JBD Bluetooth BMS up and running.
The parameters are a bit overwhelming to me, so some help would be appreciated or if there is some sort of guide online?
Anyway to get to the main points/questions:
1. I set "nominal capacity" to 37.7AH, as I have a 37.7AH52V battery is this correct?
2. Are there any other important parameters I need to set? (See pics for all the parameters)
3. Is it possible to set the max charge to approximately 90% for example?
4. On the BMS I have 2 wires coming from NTC, they look like temp sensors, am I suppose to attach these in a specific location on the battery?
Oh and the battery is running a BBSHD with the custom firmware so that's I believe 32amps max.
Pictures:
First picture battery specs from the supplier.
All other pictures from the app parameters and cell groups, looks nice and balanced.
Last picture temps sensors? Where should they be placed?









So I had battery problems and decided to get a new BMS. I'm happy that everything went well and have the JBD Bluetooth BMS up and running.
The parameters are a bit overwhelming to me, so some help would be appreciated or if there is some sort of guide online?
Anyway to get to the main points/questions:
1. I set "nominal capacity" to 37.7AH, as I have a 37.7AH52V battery is this correct?
2. Are there any other important parameters I need to set? (See pics for all the parameters)
3. Is it possible to set the max charge to approximately 90% for example?
4. On the BMS I have 2 wires coming from NTC, they look like temp sensors, am I suppose to attach these in a specific location on the battery?
Oh and the battery is running a BBSHD with the custom firmware so that's I believe 32amps max.
Pictures:
First picture battery specs from the supplier.
All other pictures from the app parameters and cell groups, looks nice and balanced.
Last picture temps sensors? Where should they be placed?









Last edited: