MitchJi
10 MW
Hi,
http://www.eurekalert.org/pub_releases/2009-04/osu-adl040809.php
http://www.eurekalert.org/pub_releases/2009-04/osu-adl040809.php
Ancient diatoms lead to new technology for solar energy
CORVALLIS, Ore. – Engineers at Oregon State University have discovered a way to use an ancient life form to create one of the newest technologies for solar energy, in systems that may be surprisingly simple to build compared to existing silicon-based solar cells.
The secret: diatoms.
These tiny, single-celled marine life forms have existed for at least 100 million years and are the basis for much of the life in the oceans, but they also have rigid shells that can be used to create order in a natural way at the extraordinarily small level of nanotechnology.
By using biology instead of conventional semiconductor manufacturing approaches, researchers at OSU and Portland State University have created a new way to make "dye-sensitized" solar cells, in which photons bounce around like they were in a pinball machine, striking these dyes and producing electricity. This technology may be slightly more expensive than some existing approaches to make dye-sensitized solar cells, but can potentially triple the electrical output.
"Most existing solar cell technology is based on silicon and is nearing the limits of what we may be able to accomplish with that," said Greg Rorrer, an OSU professor of chemical engineering. "There's an enormous opportunity to develop different types of solar energy technology, and it's likely that several forms will ultimately all find uses, depending on the situation."
Dye-sensitized technology, for instance, uses environmentally benign materials and works well in lower light conditions. And the new findings offer advances in manufacturing simplicity and efficiency.
"Dye-sensitized solar cells already exist," Rorrer said. "What's different in our approach are the steps we take to make these devices, and the potential improvements they offer."
The new system is based on living diatoms, which are extremely small, single-celled algae, which already have shells with the nanostructure that is needed. They are allowed to settle on a transparent conductive glass surface, and then the living organic material is removed, leaving behind the tiny skeletons of the diatoms to form a template.
A biological agent is then used to precipitate soluble titanium into very tiny "nanoparticles" of titanium dioxide, creating a thin film that acts as the semiconductor for the dye-sensitized solar cell device. Steps that had been difficult to accomplish with conventional methods have been made easy through the use of these natural biological systems, using simple and inexpensive materials.
"Conventional thin-film, photo-synthesizing dyes also take photons from sunlight and transfer it to titanium dioxide, creating electricity," Rorrer said. "But in this system the photons bounce around more inside the pores of the diatom shell, making it more efficient."
The physics of this process, Rorrer said, are not fully understood – but it clearly works. More so than materials in a simple flat layer, the tiny holes in diatom shells appear to increase the interaction between photons and the dye to promote the conversion of light to electricity, and improve energy production in the process.
The insertion of nanoscale tinanium oxide layers into the diatom shell has been reported in ACS Nano, a publication of the American Chemical Society, and the Journal of Materials Research, a publication of the Materials Research Society. The integration of this material into a dye-sensitized solar cell device was also recently described at the fourth annual Greener Nanoscience Conference.
The work is supported by the National Science Foundation and the Safer Nanomaterials and Nanomanufacturing Initiative, a part of the Oregon Nanoscience and Microtechnologies Institute.
Diatoms are ancient, microscopic organisms that are found in the fossil record as far back as the time of the dinosaurs. They are a key part of the marine food chain and help cycle carbon dioxide from the atmosphere.
But in recent years their tiny, silica shells have attracted increasing attention as a way to create structure at the nano level. Nature is the engineer, not high tech tools. This is providing a more efficient, less costly way to produce some of the most advanced materials in the world.
Editor's Note: The professional publication this story is based on can be found at this URL:
http://pubs.acs.org/doi/full/10.1021/nn800470x