http://www.sciencealert.com/watch-this-is-the-world-s-lightest-metal?cmpid=NL_LS_weekly_2015-10-12Watch: This is the world's lightest metal
99.99 percent air.

[youtube]k6N_4jGJADY[/youtube]
"100 times lighter than styrofoam but is as rigid as metal"
The lattice in the metal is made up of interconnected hollow metal tubes - constructed from nickel, in the case of the prototype. Each of these tubes has a wall thickness of just 100 nanometres, which is 1,000 times thinner than human hair.