Kurt
10 kW
I just picked up a Toyota prius battery pack from ebay .The pack is from a 2nd gen prius that had traveled 20,000km and is apparently in very good condition. I have a couple of questions.
I want to use them on my 48v e bike . From what info could dig up on the cells I worked out I could use 7 of the 38 modules to make a 50.4v 6.5ah pack. The modules way 1.04kg each so each 48v pack would be around 7.28kg. I would like to run two of the packs to make a 13ah 48v pack that would weigh in at 14.56 kg. My 48v sla pack is around 17kg and the weight is fine in my bob trailer.
What I am not sure about is charging the packs. I don't plan on trying to emulate the prius bms and get 1000 years use out of the battery though I don't want to kill them with the wrong kind of charger.I don't have much experience with NIMH.
At the moment the only charger i have is a sla 48 volt 1.8 amp smart charger prob no good to me now? . What kind of chargers do the e bike 48v nimh battery's come with ? What about when I try and parallel two sets of the 48v packs is nimh ok to run like this ? I remember reading something about charging nimh in parallel is a no no. I guess I could charge them individually.
Any help on making the best use of my 38 7.2v 6.5ah Nimh modules would by great.
kurt.
I want to use them on my 48v e bike . From what info could dig up on the cells I worked out I could use 7 of the 38 modules to make a 50.4v 6.5ah pack. The modules way 1.04kg each so each 48v pack would be around 7.28kg. I would like to run two of the packs to make a 13ah 48v pack that would weigh in at 14.56 kg. My 48v sla pack is around 17kg and the weight is fine in my bob trailer.
What I am not sure about is charging the packs. I don't plan on trying to emulate the prius bms and get 1000 years use out of the battery though I don't want to kill them with the wrong kind of charger.I don't have much experience with NIMH.
At the moment the only charger i have is a sla 48 volt 1.8 amp smart charger prob no good to me now? . What kind of chargers do the e bike 48v nimh battery's come with ? What about when I try and parallel two sets of the 48v packs is nimh ok to run like this ? I remember reading something about charging nimh in parallel is a no no. I guess I could charge them individually.






Any help on making the best use of my 38 7.2v 6.5ah Nimh modules would by great.
kurt.