Hugues
1 kW
UPDATE Dec. 3rd 2011: New info added on Dec. 3rd 2011, please read the newest posts below if you are interested in this tire
********************
While riding yesterday i saw some nasty icy spots along the road so today i thought i would install my new winter tires with studs.
I bought these:
http://schwalbe.com/gbl/en/produkte/tour_city/produkt/index.php5?flash=1&ID_Einsatzbereich=9&ID_Produktgruppe=36&ID_Produkt=139&ID_Artikel=78&info=1&ID_Land=38&ID_Sprache=2&tn_mainPoint=Produkte&tn_subPoint=Tour/City
Rather expensive, about 80 usd a piece, mounted a pair.
Initial riding on paved road is ok, a bit noisy but that was expected, feels like riding on a paved road with small gravel surface.
They were inflated at 60 psi, pretty much the recommended max.
Rode uphill for about 16 km, mostly paved forest roads, then some nasty trails with a mix of big rocks, mud and grass.
The grip is very good, i was impressed. Also when crossing the stream with the icy patch, no problem. Very good and secure handling.
But that's where the love story ends
I stopped for a drink after 16km uphill and checked my tires: yikes !!!! many studs are missing !!!
20 studs gone on front wheel and 56 ! at the back, that's 10% and 30 % !!!!! after 16 km of going up hill only. Bike is 30kg, with me that's 100kg.
I did not ride like crazy, just normal stuff. Pictures below.
Well, too bad, i liked the way they grip. Back to vendor this week, will see what he says.
Any recommendation for better studded tires, that can ride on paved roads and not awfully noisy ?

View attachment 1
********************
While riding yesterday i saw some nasty icy spots along the road so today i thought i would install my new winter tires with studs.
I bought these:
http://schwalbe.com/gbl/en/produkte/tour_city/produkt/index.php5?flash=1&ID_Einsatzbereich=9&ID_Produktgruppe=36&ID_Produkt=139&ID_Artikel=78&info=1&ID_Land=38&ID_Sprache=2&tn_mainPoint=Produkte&tn_subPoint=Tour/City
Rather expensive, about 80 usd a piece, mounted a pair.
Initial riding on paved road is ok, a bit noisy but that was expected, feels like riding on a paved road with small gravel surface.
They were inflated at 60 psi, pretty much the recommended max.
Rode uphill for about 16 km, mostly paved forest roads, then some nasty trails with a mix of big rocks, mud and grass.
The grip is very good, i was impressed. Also when crossing the stream with the icy patch, no problem. Very good and secure handling.
But that's where the love story ends
20 studs gone on front wheel and 56 ! at the back, that's 10% and 30 % !!!!! after 16 km of going up hill only. Bike is 30kg, with me that's 100kg.
I did not ride like crazy, just normal stuff. Pictures below.
Well, too bad, i liked the way they grip. Back to vendor this week, will see what he says.
Any recommendation for better studded tires, that can ride on paved roads and not awfully noisy ?

View attachment 1