Couple of days ago my bike fell on the ground. 48V lifepo4 vpower.
One 16s string is now wasted charge at 2.6v and idle at 1.1v. Cells are made of metal 18650 strings.
The amount of glue of this pack is terrible; I wish to avoid repair.
Would it be ok if I just doesn't care about those cell; or will they explode and ruin the whole pack if used regularly?
Thinking of bypassing the BMS for discharging or faking a good voltage for this string on the bms.
Even if it's my fault that the pack is not working; would not recommend anyone now; too much hassle to repair.
One 16s string is now wasted charge at 2.6v and idle at 1.1v. Cells are made of metal 18650 strings.
The amount of glue of this pack is terrible; I wish to avoid repair.
Would it be ok if I just doesn't care about those cell; or will they explode and ruin the whole pack if used regularly?
Thinking of bypassing the BMS for discharging or faking a good voltage for this string on the bms.
Even if it's my fault that the pack is not working; would not recommend anyone now; too much hassle to repair.