bzhwindtalker
100 kW
Some pics of our latest test bike, suspension is on point but we still have to reduce chain noise a bit, we have issues sourcing #219 drive sprokets so we have to laser cut our own out of 12mm XC70 steel and heat treat them wich makes it hard to have a good precision (=low noise)
It uses a 10S6P battery with panasonic cells and custom solderless construction. We have more testing to do on the solderless packs but we will offer beta test kits at cost in the near future.
Weight is 27.8kg, we could save 2kg by going from a 50mm stataor to a 25mm stator motor like the original GNG one, plus another few hundred grams on the components.
It uses a 10S6P battery with panasonic cells and custom solderless construction. We have more testing to do on the solderless packs but we will offer beta test kits at cost in the near future.
Weight is 27.8kg, we could save 2kg by going from a 50mm stataor to a 25mm stator motor like the original GNG one, plus another few hundred grams on the components.