Hi All,
Hoping someone can put my mind at ease about some batteries in a pack I recently purchased - here is a photo. https://goo.gl/photos/PHpFGtE4e7QMFwFy8 They are marked as NCR18650GA but are also marked 'made in china'.
This concerned me because these packs (52v 14ah shark pack) were advertised with the following notes, which the 'made in china' contradicts;
"This is the same pack loaded with panasonic cells (same cell that Tesla uses) "
"We designed these packs using a common ebike case, but filled them with quality Japanese name brand 18650 cells utilizing the latest battery chemistry to get the highest possible power density. "
"These packs have more amp hours than any commercial ebike, who skimp and use Chinese cells which are known for being low power density and short battery life. In fact we so disbelieve in Chinese cells, we are not even offering them as an option. We only offer quality cells in our packs not cheap no name Chinese cells like almost everyone else does. "
I posted at electric bike.com but didn't get an answer, although one member states GA cells aren't made in china. Thread is here:. https://electricbike.com/forum/forum/knowledge-base/batteries-aa/24645-battery-identification-what-are-these
Thanks all
Hoping someone can put my mind at ease about some batteries in a pack I recently purchased - here is a photo. https://goo.gl/photos/PHpFGtE4e7QMFwFy8 They are marked as NCR18650GA but are also marked 'made in china'.
This concerned me because these packs (52v 14ah shark pack) were advertised with the following notes, which the 'made in china' contradicts;
"This is the same pack loaded with panasonic cells (same cell that Tesla uses) "
"We designed these packs using a common ebike case, but filled them with quality Japanese name brand 18650 cells utilizing the latest battery chemistry to get the highest possible power density. "
"These packs have more amp hours than any commercial ebike, who skimp and use Chinese cells which are known for being low power density and short battery life. In fact we so disbelieve in Chinese cells, we are not even offering them as an option. We only offer quality cells in our packs not cheap no name Chinese cells like almost everyone else does. "
I posted at electric bike.com but didn't get an answer, although one member states GA cells aren't made in china. Thread is here:. https://electricbike.com/forum/forum/knowledge-base/batteries-aa/24645-battery-identification-what-are-these
Thanks all