Zoot Katz
100 kW
Something prompted me to at last enter my memo pad battery log into a spreadsheet.
It generated some numbers that might be informative.
System: X5304 R, 72V 48A Xlyte SI digital controller, 2 X 24V, 18Ah, Nexcell NiMH in series.
Bike: Mixte MTB with Xtracycle. Rider: 150 lbs. HIlly terrain. Urban traffic.
3627 kilometers
46 charge cycles
Average 14.16 amp hours per charge
Average 77.93 kilometers per charge
Average Max spd. 46.63 kmh
Average speed 17.7 kmh
Average Wh/km 8.78
It generated some numbers that might be informative.
System: X5304 R, 72V 48A Xlyte SI digital controller, 2 X 24V, 18Ah, Nexcell NiMH in series.
Bike: Mixte MTB with Xtracycle. Rider: 150 lbs. HIlly terrain. Urban traffic.
3627 kilometers
46 charge cycles
Average 14.16 amp hours per charge
Average 77.93 kilometers per charge
Average Max spd. 46.63 kmh
Average speed 17.7 kmh
Average Wh/km 8.78