Speedict neptune lite

Batteries, Chargers, and Battery Management Systems.
User avatar
Nordle   100 W

100 W
Posts: 182
Joined: Jul 20 2015 1:42pm
Location: The Alps

Re: Speedict neptune lite

Post by Nordle » Feb 25 2016 8:48am

Will model3 balance cells only when they're hitting max voltage, or balance all time? Can i set max voltage per cell? What will it cost approximately?
4:20 Noob Hubz! BLAZE it
..sry for dat poor english..

User avatar
speedict   10 kW

10 kW
Posts: 654
Joined: Jun 13 2011 11:34pm
Location: Hong Kong
Contact:

Re: Speedict neptune lite

Post by speedict » Feb 26 2016 11:29pm

good question !
Nordle wrote:Will model3 balance cells only when they're hitting max voltage
no, model3 constantly balance and compare cell delta voltage, dynamically adjust its cell release voltage, also provides 3 kind of terminations - TIMER, CELL DELTA, CV CHARGE CURRENT.
Nordle wrote:balance all time?
its depended on customer set CELL DELTA value, when BALANCE CHARGE method is selected WITHOUT charger plug-in, model 3 start CELL BALANCE immediately without charging and terminate when CELL DELTA value reached. model 3 allows customers use QUICK CHARGE, BALANCE CHARGE(with larger cell delta value) with supervisor and BALANCE only during over-night for safety consideration.

QUCK CHARGE terminate when anyone cell reached cell top voltage e.g. 4.25v

Nordle wrote:Can i set max voltage per cell?
yes, model 3 allows 0.5 margin add on top of the preset cell voltage e.g. 4.25v for lipo

Nordle wrote:What will it cost approximately?
we are collecting market information, do you have any ideas ? we are open to discuss it.

we are not expert in battery, we need customers and battery builders's feedback to improve our charging workflow and algorithm, via the firmware upgrade we can keep improve the charge efficiency :)



little background : most of the market BMS start cell discharge when cell voltage hit the fix OC voltage e.g. 4.2v then disconnect charge circuit, wait until cell reached the fix release voltage e.g. 4.1v then re-connect charge circuit to allow charge current in, the process repeat until end of CV stage (indicated by CV tiny current), sometime when CV charge current > charge preset terminate current value AND = cell discharge current, you never know when the pack is fully charge by the indicator of charger LED.
Speedict Technology - Drive . The . Future http://www.speedict.com | http://www.facebook.com/speedict.technology

User avatar
parabellum   10 MW

10 MW
Posts: 2090
Joined: Nov 19 2010 9:55am
Location: Dominican Republic, north.

Re: Speedict neptune lite

Post by parabellum » Feb 27 2016 1:39pm

There are some of us convinced (or certain) that HVC should be under 4.2V, considering chemistry and behavior of each battery type (mostly cycle life related). It can be somewhere between 4.00 to 4.15V. Sorry, I am still v4 and v5 client, but I believe, it applies for all Li bat. users. Waiting for 24s, you are a man!

Dias   10 mW

10 mW
Posts: 23
Joined: Feb 16 2016 11:48am

Re: Speedict neptune lite

Post by Dias » Mar 11 2016 3:32am

Any news about model 3 Neptune release date and estimated price? I might be interested in testing it on my build :)

User avatar
speedict   10 kW

10 kW
Posts: 654
Joined: Jun 13 2011 11:34pm
Location: Hong Kong
Contact:

Re: Speedict neptune lite

Post by speedict » Mar 15 2016 2:34am

Dias wrote:Any news about model 3 Neptune release date and estimated price? I might be interested in testing it on my build :)

we target May 2016
Speedict Technology - Drive . The . Future http://www.speedict.com | http://www.facebook.com/speedict.technology

FluxZoom   100 W

100 W
Posts: 107
Joined: Mar 25 2016 2:35am
Location: Midwest, USA

Re: Speedict neptune lite

Post by FluxZoom » Mar 26 2016 12:29pm

Very interested in model 3. What sort of time frame do you have for release?
Edit: Embarrassed, I missed looking at the second page.
Last edited by FluxZoom on Mar 27 2016 10:06am, edited 1 time in total.

davideserin   1 W

1 W
Posts: 63
Joined: Feb 01 2016 7:57am

Re: Speedict neptune lite

Post by davideserin » Mar 27 2016 6:22am

I am just about to build a 14S5P battery and would wait for the model 3 Neptune for my BMS, but what is the continuous and max current capability?

Is there also any comparison charts between the different products you make? It's difficult to see exactly what is different.

User avatar
speedict   10 kW

10 kW
Posts: 654
Joined: Jun 13 2011 11:34pm
Location: Hong Kong
Contact:

Re: Speedict neptune lite

Post by speedict » Apr 03 2016 3:58am

davideserin wrote:I am just about to build a 14S5P battery and would wait for the model 3 Neptune for my BMS, but what is the continuous and max current capability?

Is there also any comparison charts between the different products you make? It's difficult to see exactly what is different.
sorry about the late reply to this thread as we are very busy on current project !

regarding the max. discharge current we would like to control within 30A, since the current path temperature is monitored therefore if customers feel comfortable with the device temperature (either caused by rated 30A or peak 30A) we can release the discharge current control later on.

please stay turned for the product comparison detail later on ...
Speedict Technology - Drive . The . Future http://www.speedict.com | http://www.facebook.com/speedict.technology

User avatar
speedict   10 kW

10 kW
Posts: 654
Joined: Jun 13 2011 11:34pm
Location: Hong Kong
Contact:

Re: Speedict neptune lite

Post by speedict » Apr 03 2016 3:59am

Manually discharge cell # 10 to 3.76V caused cell delta to 44mV, and see if new algorithm can balance charge it back to normal ...
Attachments
before-charge-delta-44mv.png
before-charge-delta-44mv.png (21.62 KiB) Viewed 4059 times
after-charge-delta-1mv.png
after-charge-delta-1mv.png (20.34 KiB) Viewed 4059 times
Speedict Technology - Drive . The . Future http://www.speedict.com | http://www.facebook.com/speedict.technology

User avatar
Monstarr   100 W

100 W
Posts: 220
Joined: Apr 12 2011 4:56am
Location: The Netherlands

Re: Speedict neptune lite

Post by Monstarr » Apr 06 2016 5:16am

speedict wrote:Manually discharge cell # 10 to 3.76V caused cell delta to 44mV, and see if new algorithm can balance charge it back to normal ...
When will 20S + be available? I need one! :lol:
Is the iOs app still supported? I can't find it in the appstore.

FluxZoom   100 W

100 W
Posts: 107
Joined: Mar 25 2016 2:35am
Location: Midwest, USA

Re: Speedict neptune lite

Post by FluxZoom » Apr 08 2016 10:39am

speedict wrote:Manually discharge cell # 10 to 3.76V caused cell delta to 44mV, and see if new algorithm can balance charge it back to normal ...
Learn anything interesting?

I am very interested in the balancing style taken by your BMSs, what sort of approach will be taken?

I don't know names for the types of balancing, but I can think of several ways to do it but I am sure listing them in my less than knowledgable way would be a waste of time, perhaps you can just lay it out for me.

Thanks

User avatar
speedict   10 kW

10 kW
Posts: 654
Joined: Jun 13 2011 11:34pm
Location: Hong Kong
Contact:

Re: Speedict neptune lite

Post by speedict » Apr 14 2016 11:55pm

need to change the end of charge cell voltage e.g. set to 4.25V, for small capacity pack when charge mosfet turn on with pack voltage ~62.5V charge current 0.2A can immediately cut-off by cell voltage protection ...
Attachments
charge-balance-delta-0mv.png
charge-balance-delta-0mv.png (20.06 KiB) Viewed 4008 times
Speedict Technology - Drive . The . Future http://www.speedict.com | http://www.facebook.com/speedict.technology

User avatar
speedict   10 kW

10 kW
Posts: 654
Joined: Jun 13 2011 11:34pm
Location: Hong Kong
Contact:

Re: Speedict neptune lite

Post by speedict » Apr 15 2016 12:22am

extended the end of charge cell voltage or cell voltage protection to 4.25v.

open more parameters on charge option menu, such as... set the charge terminate criteria with "WHEN PACK VOLTAGE >= 63.00V" AND "CELL DELTA <= 4mV"
Attachments
eocc-425.png
eocc-425.png (21.11 KiB) Viewed 4004 times
Speedict Technology - Drive . The . Future http://www.speedict.com | http://www.facebook.com/speedict.technology

cwah   10 GW

10 GW
Posts: 4256
Joined: Jul 24 2011 5:42am
Location: Between paris and london

Re: Speedict neptune lite

Post by cwah » Apr 15 2016 2:01am

speedict wrote:Manually discharge cell # 10 to 3.76V caused cell delta to 44mV, and see if new algorithm can balance charge it back to normal ...
Is the balance charge discharging all the other cells to equilise to normal, or does it charge specifically the cell 10 (which would be better)

User avatar
speedict   10 kW

10 kW
Posts: 654
Joined: Jun 13 2011 11:34pm
Location: Hong Kong
Contact:

Re: Speedict neptune lite

Post by speedict » Apr 15 2016 7:38am

cwah wrote:
speedict wrote:Manually discharge cell # 10 to 3.76V caused cell delta to 44mV, and see if new algorithm can balance charge it back to normal ...
Is the balance charge discharging all the other cells to equilise to normal, or does it charge specifically the cell 10 (which would be better)
it is balance while charging or standalone balance, under certain circumstance individual cell charge is efficient than balance charging, when more cell in series energy transfer between adjacent cell is very hard to control (balance) without discharge mechanism, also standalone overnight cell balance is one of the recommend features.

consider charge current, individual cell charge handle charge-current via balance connector's wire vs. pack charge via #14 wire and charge current or power provided by market ready cc cv charger.

thank you cwah for the opportunity to discuss the charge method :)
Speedict Technology - Drive . The . Future http://www.speedict.com | http://www.facebook.com/speedict.technology

induna   100 mW

100 mW
Posts: 48
Joined: Mar 02 2010 11:39pm
Location: San Vito de Coto Brus, Costa Rica

Re: Speedict neptune lite

Post by induna » Apr 15 2016 4:47pm

I'm definitely interested in Model 3. Keep us posted.

User avatar
stevecgn   1 µW

1 µW
Posts: 1
Joined: Apr 24 2016 5:50pm
Location: West-Germany

Re: Speedict neptune lite

Post by stevecgn » Apr 25 2016 8:45am

Looks great!
Looking for "model 4 / 5 / 6"... as currently drive a 24 cells / 72V.... if you need a beta tester, just drop me a line 8)
Erider Thunder | 5KW | 2012 | 2500 km | GBS-LFMP-40AH | 2.89 kWh | 72 V | Kelly 72201AJ | L3e
GBS China, formerly Ningbo Thundersky. These are the first cells to have passed China's certification tests for on road use!

User avatar
speedict   10 kW

10 kW
Posts: 654
Joined: Jun 13 2011 11:34pm
Location: Hong Kong
Contact:

Re: Speedict neptune lite

Post by speedict » May 01 2016 10:34pm

<< No Fault Expedite Replacement Services >>

Over the years we have experience a number of users request for repairs services, of which, vast majority of them are not warranty related. They wish to substantially reduce the turnaround time to minimize the interruption of their daily trips. in addition, we have users whose screw up the product themselves do wish we have a more generous or substantially discounted product replacement policy.

In answer to these requests, we will introduce a “no fault expedite replacement services” to registered users, upon request, and we identified the product is qualify for an RMA, Speediest will immediate ship a new replacement product for a fixed price of (15 euros), shipping and handling included.
Speedict Technology - Drive . The . Future http://www.speedict.com | http://www.facebook.com/speedict.technology

boscovich   1 mW

1 mW
Posts: 10
Joined: Dec 12 2015 5:20am

Re: Speedict neptune lite

Post by boscovich » Jun 19 2016 9:35am

Any updates on the various models?

Sent from my GT-I9505 using Tapatalk

User avatar
markz   100 GW

100 GW
Posts: 12180
Joined: Jan 09 2014 11:38pm
Location: Canada and the USA

Re: Speedict neptune lite

Post by markz » Jul 06 2016 11:31pm

boscovich wrote:Any updates on the various models?

Sent from my GT-I9505 using Tapatalk
Yes

Any updates!?

I am interested in the Models 5 and 6.... as I run 72V nominal. But if you have to limit the discharge to 30A then I dont want that. I run 65A on my Lyen 18FET controller with A123 model M1A size 26650 battery cans. Those are very high discharge. Maybe you can have a disable feature on the discharge. But I would want a balance charge feature for sure.
Model 1 : only cell monitoring, fixed 10 - 15 cells, no cell balancing, no charge discharge control
Model 2 : cell monitoring fixed 10 - 15 cells with cell balancing, no charge discharge control
model 3 : bms features, fixed 10 - 15 cells, with cell balancing, with charge discharge controls
model 4 : only cell monitoring, fixed 12 - 32 cells, no cell balancing, no charge discharge control
model 5 : only cell monitoring fixed 12 - 32 cells with cell balancing, no charge discharge control
model 6 : bms features, fixed 12 - 32 cells with cell balancing, with charge discharge controls

tkc.87   1 µW

1 µW
Posts: 4
Joined: Sep 12 2016 6:16am

Re: Speedict neptune lite

Post by tkc.87 » Sep 12 2016 6:20am

Hello,

Exactly the same for me. I need a Model 5 or Model 6 to balance a 72V 20s battery.

When should you release it ?

mistercrash   10 kW

10 kW
Posts: 972
Joined: Mar 09 2011 11:01am
Location: Guelph, Ontario, Canada eh!

Re: Speedict neptune lite

Post by mistercrash » Sep 12 2016 7:55am

I am looking at model 4. Bluetooth is nice but I would prefer the option to plug in a very loud external alarm as a warning that something has gone astray in the battery. Any plans on offering that option? Also are the parameters of the Speedict adjustable? I would also prefer if they were. Cool product by the way, just found out about it.

Thanks
Ray

rosich   100 mW

100 mW
Posts: 49
Joined: Dec 03 2010 11:02am

Re: Speedict neptune lite

Post by rosich » May 04 2017 5:57am

Speedict has just updated their website with latest BMS product - NEPTUNE 15

tkc.87   1 µW

1 µW
Posts: 4
Joined: Sep 12 2016 6:16am

Re: Speedict neptune lite

Post by tkc.87 » May 04 2017 6:38am

Arf ... 20s will be coming soon ?

User avatar
speedict   10 kW

10 kW
Posts: 654
Joined: Jun 13 2011 11:34pm
Location: Hong Kong
Contact:

Re: Speedict neptune lite

Post by speedict » May 30 2017 5:50am

we have added one customisable cell high and low option for balance charge protection in response to customer's suggestion that according to the battery research article in order to prolong lithium battery life it should not let battery pack fully charged :)

How to Prolong Lithium-based Batteries
http://batteryuniversity.com/learn/arti ... _batteries

see attached screen captures :

1. user can select Battery Type "Custom" and select 4.10V as highest cell voltage.
2. battery pack cell delta 160mV with highest cell 4.08V before balance charging.
3. end result its cell highest cell voltage is 4.10V with cell delta 30mV.
Attachments
device option custom.png
device option custom.png (26.42 KiB) Viewed 3523 times
before charge delta 16.png
before charge delta 16.png (22.17 KiB) Viewed 3523 times
charge to 410 result.png
charge to 410 result.png (22.18 KiB) Viewed 3523 times
Speedict Technology - Drive . The . Future http://www.speedict.com | http://www.facebook.com/speedict.technology

Post Reply