B
Reaction score
4

Latest activity Postings About

    • B
      bww129 replied to the thread Luna Wolf V2 - cell voltages.
      Finally got back to working on this because it's difficult to be around for so long while each group charges, but I got to C6 and...
    • B
      bww129 replied to the thread Luna Wolf V2 - cell voltages.
      Group C1 charged up from 3.79V to 3.96V. Group C13 charged up from 2.94V to 4.07V. Charging C4 now. Seems to be working so far but...
    • B
      bww129 replied to the thread EM3ev vs Luna Batteries and Kits.
      Did you ride with me every time I used the Wolf pack? Were you in my house every time I charged the pack? The battery, and typically my...
    • B
      bww129 replied to the thread EM3ev vs Luna Batteries and Kits.
      That's a great design that will ensure higher pack capacity over a longer period of time because the cells will almost always be...
    • B
      bww129 replied to the thread Luna Wolf V2 - cell voltages.
      It's not pretty and not for the faint of heart, but if it can save the pack then it's worth it. Covering up these sections with some hot...
    • B
      bww129 replied to the thread EM3ev vs Luna Batteries and Kits.
      Hate away without any details... or read on for more information. The pack was purchased in March of 2020 and I've used it in the...
    • B
      bww129 replied to the thread Luna Wolf V2 - cell voltages.
      I first attempted to use a hot air gun to melt away the potting but it resulted in a fair amount of smoke and didn't melt it away as...
      • PXL_20240903_214150835.jpg
      • PXL_20240903_214214202.MP.jpg
    • B
      bww129 replied to the thread Luna Wolf V2 - cell voltages.
      If the manual rebalancing doesn't work I'll probably try to take the entire ABS shell off to see if any of the cell level fuses have...
    • B
      This pack was great for a couple years but has gone downhill fast. It now has very limited capacity and I had to find out why so I...
      • PXL_20240902_180917775.jpg
      • PXL_20240902_180942867.jpg
  • Loading…
  • Loading…