The 52v 14Ah battery I bought from, caught fire and burned.
Also the battery did not deliver more than 9,5 Ah, less than the promised 14Ah. Actually, none of the low cost batteries I bought from China delivered the Ah's as promised.
My next battery will come from someone who is known for...