Yes, 9 ply (6 long + 3 cross grain). The last board was 10 ply (8 long + 2 cross). 2 layers carbon. Too much, maybe. But I learned on the first board (7 layer, 1 carbon layer top), that the flex is very different with a three wheeler. Much more torsional or twist flex. The back wheel "waggled"...