    Kickbike Electric Scooter Build

    The front of the bike is pretty heavy. I originally wanted to go with rear drive and weld a custom rear rack to go over the wheel but the rear dropout spacing is only 65mm with an 18" tire. It would have been more work than I wanted to convert it to a wider dropout spacing for the motor. I...
  2. jlust286

    Your Creation's Before & After Pics

    Kickbike scooter more details here: https://endless-sphere.com/forums/viewtopic.php?f=6&t=81196
  3. jlust286

    Kickbike Electric Scooter Build

    I have been obsessing lately about making an electric bike for my wife. She does not like bicycle seats I want her to join the family for short bicycle rides. I had a great idea about making an electric scooter so she doesn't have to sit on a wedgie seat and since it is electric she could keep...
  4. jlust286

    Show Us Your Homemade Battery Housing

    Here is my homemade battery box. There is a left and right side. One overlaps the other along the center to help keep water out but it will only keep light rain and mud puddle spray out. To make this, I wrapped the frame with the batteries in plastic and clear tape. I then used about a...
  5. jlust286

    Your Creation's Before & After Pics

    My first build. I converted an old mongoose bike I bought from Wal-Mart about 12 years ago. 48v 500w Bafang BPM motor. 9ah Lifepo4 cells 16s2p.
  6. jlust286

    Bafang MOTOR CHOICE-- What is going on with the Codes/rpm

    I just received my Bafang 48v500w 201RPM rear motor kit a couple days ago from BMS battery. It took about 45 days to get it. The motor is black and engraved on the motor it says BPM 48v500w 26(16)