Does this bms balance, http://www.aliexpress.com/snapshot/6290240442.html?orderId=64171138909262.
I have 12s 5p. lifepo4
It seems to turn off when 1 cell gets to 3.65, the other cells are from 3.4 to 3.55.
When the top cell goes down to 3.5, the others are 3.25 to 3.4, the bms chargers again...