• Hello ES! We could use some help to get us past the finish line on building the new knowledgebase for the forum.
    Can you donate? Please see our fundraising page. Thank you!

18650 and 21700 4-wire Cell Holders for Cell Testing

A2D Electronics

🧲 New user
Joined
Sep 6, 2023
Messages
1
Location
Ontario
I’ve used many cell holders for battery testing but have never been fully satisfied with any of them, so I designed my own to get as many things right as possible: 4-wire contacts, airflow, alignment, connectors, and easy install and release. I'm selling kits to assemble your own cell holders.

The release mechanism allows you to push the tab to compress the spring and release the cell. Install a new cell by holding it up to the alignment cradle to get it centered every time, and releasing the tab.
All cell holders feature the same 4-pin 5mm pitch terminal block to easily swap your equipment between cell holders.

Holders are available for both 18650 and 21700 cells, in a 3D Printed 5A version or an FR4 (PCB material) 15A version with larger cell contacts.
3D printing files if you want to print your own are available through the links below.

Available through my website here: 4-wire Cell Holder - A2D Electronics
Or through Tindie: 4-wire Cell Holder for Battery Testing by A2DElectronics on Tindie

Cost varies depending on options and type ($7.50-19 USD). Shipping varies depending on location.
Located in Ontario, Canada.
 

Attachments

  • 18650 Cell Holder 5A 15A Battery Test Printed and PCB.jpg
    18650 Cell Holder 5A 15A Battery Test Printed and PCB.jpg
    2.7 MB · Views: 29
  • PXL_20230812_162251621.jpg
    PXL_20230812_162251621.jpg
    2.3 MB · Views: 30
  • PXL_20230812_172635032.jpg
    PXL_20230812_172635032.jpg
    2.7 MB · Views: 26
  • 4-wire Cell Holder Battery Testing Parts.jpg
    4-wire Cell Holder Battery Testing Parts.jpg
    3.3 MB · Views: 30
I came across these while looking for a charging solution for my 33140 LifePo4 cells and contacted A2D to inquire about modifying the design for my larger cells, which they were kind enough to remodel the 3DP version, so I ordered a couple.

Just wanted to post here to say they were great to work with and the product is pretty sweet. I'm going to pester them to see if they'll make a larger version of the PCB design, but the PETG 3DP version is quite robust and the printing is way more dialed in than in their pics.

XpLjGNn.jpeg
 
Back
Top