I've been running an LiFePo4 16s 48V 10ah kit for 2 season on my e-bike (approx 2200 miles) when my charger blew up. (I got a replacement from http://www.rechargeablelithiumpower.com/ quickly - excellent service). It charged up all the way to 53.5V, and everything seems to be fine. however I noticed that I was 2-3mph slower than usual.
I checked the cells and sure enough, 2 are dead.
My question is that I thought that the BMS should protect each cell individually, and shut it down all the way if there is one below the cut off voltage, so I wonder why the pack at all works with 2 dead cells?
Do I have a bad BMS? Is there an easy way to check?
BTW: My pack is using prismatic cells similar in size to the Foxx Lifepo4 10ah cells.
Thanks
Peter
I checked the cells and sure enough, 2 are dead.
My question is that I thought that the BMS should protect each cell individually, and shut it down all the way if there is one below the cut off voltage, so I wonder why the pack at all works with 2 dead cells?
Do I have a bad BMS? Is there an easy way to check?
BTW: My pack is using prismatic cells similar in size to the Foxx Lifepo4 10ah cells.
Thanks
Peter