VRdublove said:
Doc,
I have a Megapower 960 SR on the way in the mail. All 91 of my paired konions are fully charged to 4.2V. <<Talk about time consuming!!! My pack will be 54V fully charged and 22 ah. (13s/8p). How do you recommend I arrange the pack since I don't have access to the software that you used. Should I just make sure that all cells wired in parallel are as close in capacity as possible, or resistance? It could be a puzzle.
That's a great idea for having a 960sr! that will garanty you to get the best cells matching!
The idea is to get the SAME capacity for every 1s 8p subgroup. The closer capacity you will assemble them the most balanced will be your pack!
Ideally i would suggest you to mod your 960 charger for the "4 wire sensing" like i shown in one of my post here to alsi get the best accuracy for the internal resistance measurement.
ideally both of the capacity(C) and internal resistance (RI) are important. every subgroup should ideally be close to every other fr these two parameter.
the RI need to be calculated exactly like parallel resistor for your subgroup and the capacity like parallel cell...
The best would be for you to find in the internet a version of MAthlab and i could send you theprogram that operate with mathlab for optimysing your battery pack.
The acuracy and constancy of your cell measurement are also important and may take time.... cause ideally they should be measures at all the same temperature for finding their parameter when using the 960SR. so a room with a stable temperature would be great. Cause cells capacity vary with their temperature... Try to ventilate them with a fan pointing on them when measuring their capacity.
(dont forget that in the makita battery they are paired in parallel.. so you can consider these parallel pair like ONE CELL !!! that divide tyhe testig time by two!)
Here are the parameter that i follow for every cell test :
-------------------------------------------------------------------------------------------------
Parameter to sustain a constant absolute capacity value when measurement to match the packpack
-charge for 2each p cell group: 5.00A
-discharge current set to : 5.00A
-discharge trickle current stop: 0.10A
-discharge voltage LVC stop: 3.00V
-write on the cell: internal resistance, capacity and cell number like this on every 2p1s cell:
cell 1 3024 31
(where 31 is the RI, 3024 is the capacity and 1 is the cell number)
ex:
cell no : 1
capactié : 3024
res int : 31
Dont forget to charge them at 5.00A few hours after discharging
so when assembling your cells THEY MUST HAVE BEEN CHARGED ALL !!!
After that assemble your pack and try to follow the assembling idea that i shown in some picture on that foruim by searching for the tread about Konion !
Good luck VRdublove