Hello good folks!
I was wondering if any battery wiz out there have tried to revive LiNMCo cells. Any experience, advice etc is very welcome!
The situation is as follows:
I have managed to get hold of a shitload of 75 Ah, good quality Dow Kokam cells for free.
24s6p
About 40kWh worth to be exact..
Datasheet: http://www.xaltenergy.com/images/pdfs/datasheets/XE_Data_75HP.pdf
The only problem is (of course), that someone made a cockup of epic proportions, and as such managed to completely deplete the cells.
I'm talking sub 0.01V...
The cells were practically new and only had a few cycles on them, if any at all.
I have tried bulk-charging 8 cells today at sub 1/20 c, and for now at least the cells seem to be holding charge. I stopped @~3,4V out of respect for my life..
Am I an utter shitlord for even attempting this?
Would it be worth it to revive them (if possible), or am I either way sitting on a metric buttload of lithium waiting to dendrite-selfdestruct?
It's a great modular system, and I even have the BMS for them. Love the thought of all the projects I could do with this, but I'm really sceptical due to the amount of energy involved.
Hopefully I posted this in the right place! If not, please let me know.
Regards
varntzberg
I was wondering if any battery wiz out there have tried to revive LiNMCo cells. Any experience, advice etc is very welcome!
The situation is as follows:
I have managed to get hold of a shitload of 75 Ah, good quality Dow Kokam cells for free.
24s6p
About 40kWh worth to be exact..
Datasheet: http://www.xaltenergy.com/images/pdfs/datasheets/XE_Data_75HP.pdf
The only problem is (of course), that someone made a cockup of epic proportions, and as such managed to completely deplete the cells.
I'm talking sub 0.01V...
The cells were practically new and only had a few cycles on them, if any at all.
I have tried bulk-charging 8 cells today at sub 1/20 c, and for now at least the cells seem to be holding charge. I stopped @~3,4V out of respect for my life..
Am I an utter shitlord for even attempting this?
Would it be worth it to revive them (if possible), or am I either way sitting on a metric buttload of lithium waiting to dendrite-selfdestruct?
It's a great modular system, and I even have the BMS for them. Love the thought of all the projects I could do with this, but I'm really sceptical due to the amount of energy involved.
Hopefully I posted this in the right place! If not, please let me know.
Regards