cassschr1
10 kW
hey guys,give me your thoughts on this. Pack size 6x11x3. Consists of 12 konin 3ah packs,copper strips are .025 thick,6" long. Blue spade connectors are for depiction only but can be used for balancing. This is not soldered up yet.I am concerned about the" cells in parallel before series" thing but this is the same thing isn't it? Building it this way gives a 60v batt for regular controllers and 120v plus for Lyens controller. capicaity will be 11ah each pack.Charging with a meanwell at 60v or in series for 120. Can also ch with FMA powerlab 8 for balancing. JPG[/attachment]