• Hello ES! We could use some help to get us past the finish line on building the new knowledgebase for the forum.
    Can you donate? Please see our fundraising page. Thank you!

CA owners - what Ah / Wh are you getting from your battery?

rsilvers

Regular
Joined
Aug 8, 2015
Messages
339
Location
USA
What is your batteries rated capacity, number of cycles, and what does your CA indicate for Ah and WH?

I will start:

AliExpress K-Battery/Samsung 48v, 20AH,
CA: 17.3Ah, 820Wh, Rbatt 0.129Ω, Cycles 2.

IMG_0477.jpg

IMG_0478.jpg

IMG_0479.jpg

IMG_0480.jpg

IMG_0481.jpg

IMG_0482.jpg
 
Back