nickceouk
🔋 Established
- Joined
- Jan 18, 2020
- Messages
- 86
Live eBay auction here
I am selling 13 used EIG 20ah cells and a 14s BMS(30A charge/discharge)
Average 16 mohm
The cells have been unused for over an year and have been used for an ebike setup before 4 cells of the 13 were separately used for lighting setup.
Always used the cells with BMS and never used outside of 3.4v - 4.1v range. They hold charge and are good cells but I do not need them now.
Please refer to photo with cells voltages on each cell. First 9 cells are at 3.75volts and the last 4 vary slightly due as mentioned above they were used for powering lighting circuit. The voltage can be equalized by charging 3 of the cells individually to 3.75volts and discharging cell #13 to 3.75volts.
Happy to answer your questions.
Happy bidding!!!
I am selling 13 used EIG 20ah cells and a 14s BMS(30A charge/discharge)
Average 16 mohm
The cells have been unused for over an year and have been used for an ebike setup before 4 cells of the 13 were separately used for lighting setup.
Always used the cells with BMS and never used outside of 3.4v - 4.1v range. They hold charge and are good cells but I do not need them now.
Please refer to photo with cells voltages on each cell. First 9 cells are at 3.75volts and the last 4 vary slightly due as mentioned above they were used for powering lighting circuit. The voltage can be equalized by charging 3 of the cells individually to 3.75volts and discharging cell #13 to 3.75volts.
Happy to answer your questions.
Happy bidding!!!
Attachments
-
IMG20240329140809.jpg2.6 MB · Views: 13 -
IMG20240329140650.jpg2.6 MB · Views: 11 -
IMG20240329140423.jpg4 MB · Views: 11 -
IMG20240329140548.jpg3.2 MB · Views: 11 -
IMG20240329140603.jpg3.2 MB · Views: 14 -
IMG20240329140520.jpg3.1 MB · Views: 12 -
IMG20240329140624.jpg3.1 MB · Views: 16 -
IMG20240329140633.jpg2.9 MB · Views: 12
Last edited: