A excellent product would be Sprayon red insulating varnish. I sprayed my motor with this varnish, and drove all winter and there is no rust on any of the stator or magnets. It cost about 10.00 CDN/US. If you use this put on a THIN coat because if too thick the wheel will not rotate freely. as the clearence between the stator and magnets is very close.