w0ss
1 µW
- Joined
- Jan 1, 2017
- Messages
- 2
I came across some new old stock fullriver cells. They are 26650 rated at 3300mah. I put them on my B6 but they are only showing ~1ah capacity after a few charge/discharges. All the cells I took out of the box showed 3.2 volts. The outer box has 1 2012 manufacturing date.
I can't find much info on these cells does anyone have info? Also would it be likely that there is any hope for these cells? I took the risk as it was just over 1$ a cell. I was hoping they would have at least 2ah per cell. The B6 ony charges them to 3.6 with it's "3.3v life" setting. I am wondering if these need a higher voltage to fully charge.
Thanks,
WIll
I can't find much info on these cells does anyone have info? Also would it be likely that there is any hope for these cells? I took the risk as it was just over 1$ a cell. I was hoping they would have at least 2ah per cell. The B6 ony charges them to 3.6 with it's "3.3v life" setting. I am wondering if these need a higher voltage to fully charge.
Thanks,
WIll