The local insurance salvage has the battery pack from a 2010 GMC dual mode hybrid. I have found very little about this other than it is 300V NiMh battery and apparently weighs in at about 300Lbs. The reserve is $400 and the auction closes wed am. if nobody bids, then they will lower the reserve and rebid it next week. I am thinking if it can be reordered to lower the voltage it may make a good pack for an e-motorcycle. Does anybody have any knowledge about this thing?
 