Here is the specifications:


  • 40152(3.2V15Ah) lithium battery cell, widely used for electric vehicles, with the long cycle life and wonderful function

    Nominal capacity: 15000mAh (0.5c)
    Nominal voltage: 3.2V
    Internal resistance: ≤8mΩ
    Max charge current: 3C(45A)
    Max charge voltage: 3.65±0.05V
    Max discharge current: 10C(150A)
    Cut-off voltage: 2.0V
    Dimension: Diameter 40±1mm, Height 152 ±1mm
    Weight: about 480g
    Operate Temperature: Charge 0~45°C, Discharge -20~60°C
    Storage time: One month -20~45°C, Six month -20~35°C