I recently bought a spot welder for my 10S2P 21700 battery pack, I'm using 400A 12V car battery. Also I'm using 0.15x10mm nickel strips.
The issue is that welds are weak (0.1mm are fine), but the thing is after 4-5 welds welding "prongs" and wires get noticeably warm to the touch (wires are 12AWG, 50cm in total). My question is are the wires to thin/long i.e. should I double them (since 12AWG is all I have)?