EVDragRacer
1 kW
- Joined
- Dec 10, 2010
- Messages
- 318
K2 LFP 42 AH 3.2 Volt Module (LFP 165S 41.6AH Power Module)
16 - 2.6AH cells (26650P) in parallel.
2400 amps Burst Rating!
K2 LFP 73 AH 3.2 Volt Module (LFP 300HPS 72.8AH Power Module)
28 - 2.6AH cells (26650P) in parallel.
4200 amps Burst Rating!
http://www.k2battery.com/products-26650P.html
http://batteryworkshop.msfc.nasa.gov...App_JHodge.pdf
______________________________________________________________
I am researching new battery producers because we are building a second EV Drag Funny Car!
This is not the Haiyin sponsored car, this car will be built with a Funny Car Cage etc....
Haiyin would only sponsor one car, and I thank them for that!
K2 Energy posts on their website these modules are made with their:
LFP26650P Hi Power 3.2v 2.6ah cells.
http://www.k2battery.com/battery-packs.html
We all know K2 Energy gets their cells from:
DLG Power Battery (Shanghai China)
BUT, I have researched their website and find only:
LFP26650P Hi Power 3.2v 2.4ah cells ????????
________________________________________________________________
Questions are:
Is this the same cell?
or
Is DLG producing a special battery for K2 Energy?
_________________________________________________________________
I also cannot find the power modules on DLG's website?
_________________________________________________________________
I looked up K2 Energy address on Google Maps and found only a small office,
does K2 have a production facility in USA or is everything made in China?
16 - 2.6AH cells (26650P) in parallel.
2400 amps Burst Rating!
K2 LFP 73 AH 3.2 Volt Module (LFP 300HPS 72.8AH Power Module)
28 - 2.6AH cells (26650P) in parallel.
4200 amps Burst Rating!
http://www.k2battery.com/products-26650P.html
http://batteryworkshop.msfc.nasa.gov...App_JHodge.pdf
______________________________________________________________
I am researching new battery producers because we are building a second EV Drag Funny Car!
This is not the Haiyin sponsored car, this car will be built with a Funny Car Cage etc....
Haiyin would only sponsor one car, and I thank them for that!
K2 Energy posts on their website these modules are made with their:
LFP26650P Hi Power 3.2v 2.6ah cells.
http://www.k2battery.com/battery-packs.html
We all know K2 Energy gets their cells from:
DLG Power Battery (Shanghai China)
BUT, I have researched their website and find only:
LFP26650P Hi Power 3.2v 2.4ah cells ????????
________________________________________________________________
Questions are:
Is this the same cell?
or
Is DLG producing a special battery for K2 Energy?
_________________________________________________________________
I also cannot find the power modules on DLG's website?
_________________________________________________________________
I looked up K2 Energy address on Google Maps and found only a small office,
does K2 have a production facility in USA or is everything made in China?