i know you're supposed to put lipos in storage mode when leaving them in storage...but a few years ago i moved and most of my stuff was in storage. life got really busy (new city, new job, more kids, etc.) and to make a long story short, i am only now getting to my lipos.
most of these lipos were stored at around 3.9-4.0v and it's been around 3 years since they have been charged. a few were brand new at the time so they were shipped from hobbyking and haven't been touched since.
i checked the voltage of the cells via the balance tabs and it looks like most of these cells are still charged up.
my plan is to run each of these lipos through about 3 cycles of discharge/charge at 1c and observing the cells throughout the process to ensure that there isn't any odd behavior. this will happen per cell in the fireplace for safety. if i deem the lipo good, i'll use it but keep a close eye on it.
does that sound like a good approach? or is this a futile effort and should i just get rid of all of them and buy new ones?
i did find one brand new 4s 5ah turnigy hardcase that had one bad cell (0.7v). i was thinking of taking that one outside onto the cement and slowly charging it up at 0.1a to see what happens...is that really stupid?
RVD.
most of these lipos were stored at around 3.9-4.0v and it's been around 3 years since they have been charged. a few were brand new at the time so they were shipped from hobbyking and haven't been touched since.
i checked the voltage of the cells via the balance tabs and it looks like most of these cells are still charged up.
my plan is to run each of these lipos through about 3 cycles of discharge/charge at 1c and observing the cells throughout the process to ensure that there isn't any odd behavior. this will happen per cell in the fireplace for safety. if i deem the lipo good, i'll use it but keep a close eye on it.
does that sound like a good approach? or is this a futile effort and should i just get rid of all of them and buy new ones?
i did find one brand new 4s 5ah turnigy hardcase that had one bad cell (0.7v). i was thinking of taking that one outside onto the cement and slowly charging it up at 0.1a to see what happens...is that really stupid?