Hello all. I'm working in my first ebike and my first battery pack.
This is a 16s 8p 18650 panasonic 2900 mAh. Total 23.2 Ah and 67.2 Volts.
Here I explain how I built it:
My old freeride bike (15 years?)

You can see that it has a reinforcement in the center of the frame. This is a complication and forces me to split the battery pack in two (and put the BMS out of the pack).
I decided to use PVC profiles to isolate and reinforce the battery pack.
Steps:
1.- Glued and isolating each 8 cells in a package. Fixing with hot glue and american tape.

2.- Preparing nickel strips.
Flux in nickel strip to weld bms wire (with tin).

Welded cooper wire in nickel strip (first weld all wires before weld strip on cells for prevent overheat in cells).

Preview...
.
To be continue...
This is a 16s 8p 18650 panasonic 2900 mAh. Total 23.2 Ah and 67.2 Volts.
Here I explain how I built it:
My old freeride bike (15 years?)

You can see that it has a reinforcement in the center of the frame. This is a complication and forces me to split the battery pack in two (and put the BMS out of the pack).
I decided to use PVC profiles to isolate and reinforce the battery pack.
Steps:
1.- Glued and isolating each 8 cells in a package. Fixing with hot glue and american tape.

2.- Preparing nickel strips.
Flux in nickel strip to weld bms wire (with tin).

Welded cooper wire in nickel strip (first weld all wires before weld strip on cells for prevent overheat in cells).

Preview...

To be continue...