jatgm1
10 W
never buy from all-lifepo4. first they shipped me a broken charger then after a month the battery only had enough charge to get up my driveway. the BMS on these look like shit, they are litterally duct taped together and the bms is not attached to the battery in a way it cannot move but you cannot disconnect it. its the most useless peice of crap i have ever ordered and next time i will not use them. in fact i hope their company goes into debt, i wasted over 400$ on their 20ah 48v battery and it shit out in less than a month. useless. pathetic. never use them. this is a warning. p.s. the polarity of the battery was backward. the red was negitive and the black was positive the only reason i knew that is because my multimeter told me and if i just assumed it was wired normally my motor controller would have potentially lit my entire house on fire.