The Panasonic BMS photo is cropped, go to this link: http://www.pedelecforum.de/forum/attachment.php?attachmentid=30333&d=1368876155 to see it full size with the balancer plugs.
osa57 said:it's good you noticed that....
actually I have posted this video on youtube, so when I got the (strange) URL back after the end of the upload I haven't noticed that
I guess when you say:
"i have seen 6S packs with two cells at 0V and one at 4.5V. the other 3 were still working. just deformed by the puffers."
you refer to battery packs that have not been balanced/charged recently.
May be I am wrong , but if I keep doing systematically 'balance-charge' my LiPO's, the chances that while using them one cell suddenly drops under 2.7 V is extremely low.
I have been doing this for the last 3 or 4 months, and each time I didn't notice more than 0.06/0.07 Volts difference amongst cells.
I will keep an eye on how this gap goes on, whether it increases or may be decreases thanks to the balancing exercise.
osa57 said:After 3 years and almost 10000 km, both my 5800 mAh Zippy batteries are still in excellent shape
Every time I recharge them, they are (almost) perfectly balanced.
I normally charge them in parallel, so the complete recharge ( having set the Lipo charger at 10Ah) takes one hour at most.
I never let the single cell voltage drop below 3.5 Volts (thanks to the Cycle analyst).
Hi,redcap said:Hello Daniele
osa57 said:After 3 years and almost 10000 km, both my 5800 mAh Zippy batteries are still in excellent shape
Every time I recharge them, they are (almost) perfectly balanced.
I normally charge them in parallel, so the complete recharge ( having set the Lipo charger at 10Ah) takes one hour at most.
I never let the single cell voltage drop below 3.5 Volts (thanks to the Cycle analyst).
I am trying to do the same as you, I would like to replace the battery for my wife's used Flyer (26V)
Because you had success in bypassing the BMS I would like to ask if you needed to connect the battery state pin to the battery case.,.............
Thank you so much for any pointers.
Luis