Hi,
I am currently planning two 1000Wh 48V battery packs with 18650 cells
with safe chemistry like LiMnO or LiNiMnCoO.
I read about cheap BMS malfunctions, damaging cells or even catching fire.
Using safe chemistry cells together with an "unsafe" china BMS does not make much sense, right?
The goal would be "no worries" battery packs which could sit unattended for weeks
and be used daily without having to disconnect the BMS or connect external balancing charger
everytime... (not-so-easy-to-open water resistant case)
Do you have any recommendations for a reliable good quality 13 - 24S BMS (only 13S used)?
Discharge current 40A continuous, max. 60A for a few seconds (but higher is better 8) ).
Size of the board is not critical, but it should be rather thin (<30mm).
Bonus would be a digital interface for readout (RS232/485 or so), but this is not too important.
Does not have to be cheap, I'd say max. $300.
Would be great if I could avoid creating my own board...
(which I could, but is lots of work for just two boards and there are so many other things to do
)
Thanks!
I am currently planning two 1000Wh 48V battery packs with 18650 cells
with safe chemistry like LiMnO or LiNiMnCoO.
I read about cheap BMS malfunctions, damaging cells or even catching fire.
Using safe chemistry cells together with an "unsafe" china BMS does not make much sense, right?
The goal would be "no worries" battery packs which could sit unattended for weeks
and be used daily without having to disconnect the BMS or connect external balancing charger
everytime... (not-so-easy-to-open water resistant case)
Do you have any recommendations for a reliable good quality 13 - 24S BMS (only 13S used)?
Discharge current 40A continuous, max. 60A for a few seconds (but higher is better 8) ).
Size of the board is not critical, but it should be rather thin (<30mm).
Bonus would be a digital interface for readout (RS232/485 or so), but this is not too important.
Does not have to be cheap, I'd say max. $300.
Would be great if I could avoid creating my own board...
(which I could, but is lots of work for just two boards and there are so many other things to do