When the battery reaches 100% charge (on display) the BMS protection is triggered, disconnecting the power output to the controller, but the charger continues charging (at least it doesn't turn off). When I disconnect the charger, the scooter shuts down completely. According to the rules, the charger should be disconnected, but the BMS should not go into protection mode.
All 10 cells are balanced to 0.02 volts. 36V 10S 4P pack. Thermistors - 11-12 kOhm. When charge, app works, show all info. BT latest, FW actual.
All 10 cells are balanced to 0.02 volts. 36V 10S 4P pack. Thermistors - 11-12 kOhm. When charge, app works, show all info. BT latest, FW actual.