Taswegian said:More info needed, it depends what you mean by high amps.
What is the full spec of the bike and how big a pack are you willing to use?
What kind of cycle life are you hoping to see?
etc etc
IMO, for 18650 cells:ebike11 said:Hi guys..
Would like to get some opinions on brand/model cells that can put out high continuous amps
j bjork said:Samsung 20s, sony vtc5A, molycell p26, LG HB2, HB3, HB6
Check rewevs on those.
ebike11 said:j bjork said:Samsung 20s, sony vtc5A, molycell p26, LG HB2, HB3, HB6
Check rewevs on those.
What can a Samsung 20s10p 72v pack with 25R cells put out for max. continuous amps?
Haggan90 said:ebike11 said:j bjork said:Samsung 20s, sony vtc5A, molycell p26, LG HB2, HB3, HB6
Check rewevs on those.
What can a Samsung 20s10p 72v pack with 25R cells put out for max. continuous amps?
Around 200A
goatman said:did you mean the bms is 100 amps? if so you can split the pack and parallel the two 5p packs together using two bms gives 200 amps. if your thinking 25r you might consider the 30q at 12p
ebike11 said:goatman said:did you mean the bms is 100 amps? if so you can split the pack and parallel the two 5p packs together using two bms gives 200 amps. if your thinking 25r you might consider the 30q at 12p
No I cant split it.
Yes em3ev said the BMS can handle 100A.
But if the cells can handle 200A, then how could I get that extra power?
pahorpet said:I have already made this kind of batery pack and now I am building again with 30Q exacly 22s26p it would produce 92.4V and 300A continuous ofcourse with BMS, but while you run at 300A you will produce a lot of heat to cool down but for sprint it should be ok. When I will finish it I can post it than. Last time I uave made 22s40p with GEB2500mAh, 10A max. and I am using them with same setting - 300A max.
So for capacity/current/price is 30Q good choice. But for only less capacity=less weight, only sprints Lipo will do better job.
Hillhater said:Easier to help if you gave us some actual numbers you want to achieve.
ebike11 said:Ive reading up on here and ive seen posts saying that having a pack with lipo cells will generally be more powerful at the same voltage as 18650.
Im looking for high voltage and high amp capability