Toyota reduced rare earth materials magnets by 50%

LockH

1 PW
Joined
Jul 9, 2013
Messages
17,544
Location
Ummm.. Started out in Victoria BC Canada, then sta
Toyota has reduced the rare earth materials used in electric vehicle magnets by 50%:
https://www.nextbigfuture.com/2018/...s-used-in-electric-vehicle-magnets-by-50.html

Starts:
Toyota has developed the world’s first neodymium-reduced, heat-resistant magnet. Neodymium magnets are used in various types of motors such as the high-output motors found in electrified vehicles, use of which is expected to increase rapidly in the future. The new magnet uses significantly less neodymium, a rare-earth element (“rare earth”), and can be used in high-temperature conditions.

The newly developed magnet uses no terbium (Tb) or dysprosium (Dy), which are rare earths that are also categorized as critical materials necessary for highly heat-resistant neodymium magnets. A portion of the neodymium has been replaced with lanthanum (La) and cerium (Ce), which are low-cost rare earths, reducing the amount of neodymium used in the magnet.

8)
 
Back
Top