I have seen a lot of posts about the yesa and ping packs and wanted to see what everybodies thoughts are on them. I am referring to the LiFePO4 packs sold on ebay. I know many people love the ping packs and I just wanted to know how the yesa packs stack up.
The Yesa lifePO4 36v 10ah pack has 12 cells in series, 10Ah each, at 3.2V. Would anybody know what the ping packs have so we can compare?