FYI here are a few details on how I built my packs (10S1P for a 36V trike project, and a 3S3P for an e-powered kayak). I used a BMS for one pack, the 10S I did not bother (I monitor each cell with a pair of 5S RC voltage monitors/alarms). I charge them with my bench power supply dialed in at 41.0V and 3Amps for the 10S pack.
I paid about $6/cell. Capacity tests out to almost 9AH/cell.
https://www.ebay.com/itm/20-SPIM08HP-3-7V-8AH-LITHIUM-POLYMER-BATTERIES-25C-200A-SUPER-CELLS-24V-36V-48V/173305036284?hash=item2859c8fdfc:g:QXIAAOSw8~5a72gx:sc:FedExHomeDelivery!34442!US!-1:rk:3f:1&frcectupt=true
I've built two packs now. Based on my own observed performance and reliability, I am not concerned w/ their quality. I'm told they were used in a prototype bus and have few cycles on them. Also the seller is well known and respected in the DIY battery community.
View attachment 3
I paid about $6/cell. Capacity tests out to almost 9AH/cell.
https://www.ebay.com/itm/20-SPIM08HP-3-7V-8AH-LITHIUM-POLYMER-BATTERIES-25C-200A-SUPER-CELLS-24V-36V-48V/173305036284?hash=item2859c8fdfc:g:QXIAAOSw8~5a72gx:sc:FedExHomeDelivery!34442!US!-1:rk:3f:1&frcectupt=true
I've built two packs now. Based on my own observed performance and reliability, I am not concerned w/ their quality. I'm told they were used in a prototype bus and have few cycles on them. Also the seller is well known and respected in the DIY battery community.
View attachment 3