I guess i won't be needing this anymore :D
image.jpeg
It used to be a Kelly kls7230 controller, it shut itself off 3 times on the way to work, then it was completely dead when i was heading home again. I'm glad the whole bike didn't catch fire.

I wonder why it blew..

image.jpegimage.jpegimage.jpeg
FET seem to be marked K100E10NE
Could be this Toshiba FET:
View attachment TK100E10N1_datasheet_en_20140630.pdf
Does anyone know how performance is for this FET compared to the best?
Is it a good one?
 
KLS6035
Corroded inside.
In my case green stuff caused just failure (short circuit of output cascade.
rps20180131_231443.jpg
 
That's some pretty nasty corrosion. Couldn't find any signs of that or even moisture in my controller. The day i was riding was dry so i guess it was a fault just in controller design or manufacturing.

I will check the other kelly i have that stopped working, maybe it looks the same inside. That was used with another motor so if there's same fault then they could be connected to same root cause.
 