ok - so here are the voltages measured - kind of displayed in a table that mimics the batteries:
2.49, 2.9, 3.11, 3.16
3.05, 2.95, 3.07, 2.95
3.07, 3.07, 3.02, 3.15
I'm not sure what the expected range is, however that first one is low no?