Hi All, My first post. I'm not a battery expert but thought I would post what I have discovered so far. I just finished building a 2010 Norco Fluid 2.0 with Baserunner and Bafang G310 from Grin Technologies. I'm using 2 DBC210 batteries in series to give me nominal (is that the right word??) 40V. These batteries came in my DeWalt lawn mower, so making dual use. Baserunner reports 40.1 ish volts. Initial performance of the batteries seems good. Did a minor disassembly of one battery to find that the cells used are Samsung INR21700 50S 5000mah. These cells don't seem to have good life time with respect to retaining capacity after many cycles. It's ok for me thought because my bike is not a daily commuter. The cells are fused at 80A and the high power connections are all spot welded instead of soldered. I will update this post after I have put some miles on the bike (like after the snow leaves here is Langley BC) lol.