I want some feedback how my ping 48v 15ah batt is going.
My bike is a large MBT with thick steel frame weighs around 43kgs 95bs with battery Magic pie motor and accessories, today towing a 10kg (22lb) trailer with a 10yo boy in the back, he is slight build and maybe weighs only 20kgs (44lbs) I weigh 75kgs 165lbs.
Total weight, 148 kgs (326lbs.)
My back tire was a "little" flattish and forgot to test it on the pressure gauge, I went for the longest ride I do today and the wind was pounding much stronger than usuall and trees were tempestuosly swaying in the gusts, I face very little hills on my journey. I must of rode 20km (9.3mi) against the wind, maybe 15kms directly against the wind, and 5kms (3 mi) at an angle, My controller is set for 30 amps cont. And on the way home, was shorter and there was no wind at all, as it had stopped. So I estimate about 15km with no wind.
No pedals.
I made it but 500 meters from home and it started slowing a cutting out. I charged about 17.5 ah before one light on my BMS over the runt cell got switched on. and 10 minutes transpired charging at 2 amps before the all came on, maybe less amps at the end of charging cycle.. Usually all the lights come on within 10 seconds.
The pack is 22mths old and has been riden hard up to 15km-20km 7 trips a week often towing home a ton of stuff and I would usually do 9ah. On average about 662 3/4 dod cycles running @2c cont max discharge current.
I think the pack is still up to the task, but I might have to reduce the current draw to 1.5c.
So what shape do people here think my ping batt is in?
I think it did pretty good today as I havent really pushed it this hard for this distance before.
My Mrs isnt so optimistic though. She rides at max 14kms with a Low,medium load and drills it very hard 14kms from the Shops home.
My bike is a large MBT with thick steel frame weighs around 43kgs 95bs with battery Magic pie motor and accessories, today towing a 10kg (22lb) trailer with a 10yo boy in the back, he is slight build and maybe weighs only 20kgs (44lbs) I weigh 75kgs 165lbs.
Total weight, 148 kgs (326lbs.)
My back tire was a "little" flattish and forgot to test it on the pressure gauge, I went for the longest ride I do today and the wind was pounding much stronger than usuall and trees were tempestuosly swaying in the gusts, I face very little hills on my journey. I must of rode 20km (9.3mi) against the wind, maybe 15kms directly against the wind, and 5kms (3 mi) at an angle, My controller is set for 30 amps cont. And on the way home, was shorter and there was no wind at all, as it had stopped. So I estimate about 15km with no wind.
No pedals.
I made it but 500 meters from home and it started slowing a cutting out. I charged about 17.5 ah before one light on my BMS over the runt cell got switched on. and 10 minutes transpired charging at 2 amps before the all came on, maybe less amps at the end of charging cycle.. Usually all the lights come on within 10 seconds.
The pack is 22mths old and has been riden hard up to 15km-20km 7 trips a week often towing home a ton of stuff and I would usually do 9ah. On average about 662 3/4 dod cycles running @2c cont max discharge current.
I think the pack is still up to the task, but I might have to reduce the current draw to 1.5c.
So what shape do people here think my ping batt is in?
I think it did pretty good today as I havent really pushed it this hard for this distance before.
My Mrs isnt so optimistic though. She rides at max 14kms with a Low,medium load and drills it very hard 14kms from the Shops home.