Hi group...I'm new to this game and hoping I can benefit from your experience

I want to replace a bad battery in my ebike. It's 72v Li ion. The motor us 3000w and draws 47a. I have a quote from China for a 60 ah, 72v battery but it's LiPo packs in a container with management system. I don't know much about the lithium battery but I hear that the LiPo can be unstable and fussy charging. Is this battery suitable for an ebike and will it stand up to a few bumps? My present battery craps out at 11ah. I have space and want the 60ah for range

Appreciate your help, thanks
 
If they mean RC LiPo don't get that unless you specifically want it. It's more finicky and a china-made (or em3 or whatever) pack with decent 18650s will have more watt hours for a given weight and size.
 