Hi
It's been a while, and I finally got some time to tinker with my e-bike.
I also received 10 used laptop batteries that I will be ussing in addition to my other 18650 cells.
The laptop batteries are configured in 3s2p and seems to be in ok shape.
I have been testing the packs in their stock form, and inspected the oem welds. They seem good enogh.
Is there any reason I should not use the packs in their original form, remove plastic and add cables? (balance leads and "mains"), I will
The battery packs are for my 24v 250 w hub motor that I have tested at 6s-9s (low Ah packs) . with an older setup. I will probably run 8s or 9s until thing starts to break.
It's been a while, and I finally got some time to tinker with my e-bike.
I also received 10 used laptop batteries that I will be ussing in addition to my other 18650 cells.
The laptop batteries are configured in 3s2p and seems to be in ok shape.
I have been testing the packs in their stock form, and inspected the oem welds. They seem good enogh.
Is there any reason I should not use the packs in their original form, remove plastic and add cables? (balance leads and "mains"), I will
The battery packs are for my 24v 250 w hub motor that I have tested at 6s-9s (low Ah packs) . with an older setup. I will probably run 8s or 9s until thing starts to break.