ElectricBikeNoob
10 W
What are battery charging rules, guidelines, suggestions for a Samsung downtube battery?
1. Rated capacity: 10AH
2. Voltage: 48V
3. Charging Voltage: 54.6V
4. Discharge cutoff voltage: 35.75V
5. Cell: Samsung 18650 (13S4P)
6. Standard charging: 0.2C constant current(CC) charge to 54.6V, then constant voltage (CC) 54.6V charge till charge current decline to ≤0.05C
7. Continuous discharge current: 15A
8. Pulse/Max discharge current 30A
9. Max charging current : 5A
10. Charging temperature: 0~45℃
11. Dischargeing temperature: -20~55℃
12. Diamesion: 130x90x350mm
13. It has a 5V USB output for charging cell phone or ipad
Charger information
1. Charging voltage: 54.6V
2. AC input: 90V~120V or 220V~240V
3. Charging current: 2A
Should it be fully discharged before charging again? How is overcharging it too?
1. Rated capacity: 10AH
2. Voltage: 48V
3. Charging Voltage: 54.6V
4. Discharge cutoff voltage: 35.75V
5. Cell: Samsung 18650 (13S4P)
6. Standard charging: 0.2C constant current(CC) charge to 54.6V, then constant voltage (CC) 54.6V charge till charge current decline to ≤0.05C
7. Continuous discharge current: 15A
8. Pulse/Max discharge current 30A
9. Max charging current : 5A
10. Charging temperature: 0~45℃
11. Dischargeing temperature: -20~55℃
12. Diamesion: 130x90x350mm
13. It has a 5V USB output for charging cell phone or ipad
Charger information
1. Charging voltage: 54.6V
2. AC input: 90V~120V or 220V~240V
3. Charging current: 2A
Should it be fully discharged before charging again? How is overcharging it too?