whatever
100 kW
- Joined
- Jun 3, 2010
- Messages
- 1,297
I'm still using cobalts after many years on ebikes, I've had a few fires, there are some simple things can be done:
1. assume your going to have a fire at some stage is a good starting point design everything from that viewpoint
( solar challenge did not allow iron phosphates for some time........odd)
2. arrange the pack accordingly so that its not possible for one pack to heat another pack ( even a small gap may be enough to prevent spreading of heat to next pack)
3. arrange cells so that if a firecracker goes off the direction of the flame is not going to hurt driver or other cells. The cells I've been using are 5ahr in metal case, the fire always comes out the end of the cells in a certain direction.
4. packs should be able to be removed very very quickly, my experience is there is a gap between cells going off, you dont want to be moving a burning pack, extremely good chance of getting burned, but removing good packs whilst another is burning is possible ( i've done it!)
To completely burn a 100k value car is completely avoidable scenario, and expensive lesson for them .
1. assume your going to have a fire at some stage is a good starting point design everything from that viewpoint
( solar challenge did not allow iron phosphates for some time........odd)
2. arrange the pack accordingly so that its not possible for one pack to heat another pack ( even a small gap may be enough to prevent spreading of heat to next pack)
3. arrange cells so that if a firecracker goes off the direction of the flame is not going to hurt driver or other cells. The cells I've been using are 5ahr in metal case, the fire always comes out the end of the cells in a certain direction.
4. packs should be able to be removed very very quickly, my experience is there is a gap between cells going off, you dont want to be moving a burning pack, extremely good chance of getting burned, but removing good packs whilst another is burning is possible ( i've done it!)
To completely burn a 100k value car is completely avoidable scenario, and expensive lesson for them .