You will have no issues.
I run a pair of 10s 8ah Graphene lipo's in parallel and then in parallel with a 10s 13ah samsung li-on pack and they behave very well, voltage discharge will remain fairly equal, just make sure the voltages are similar when you connect. If the voltages are a bit out then you will get a rush of amps flowing as the cells/packs equalise the wiring will get warm or very warm if volts are far apart. Big discrepencies of voltage between packs may cause wiring/connectors to melt if underated.
After yesterdays ride my 13ah had end Voltage 37.25 and the lipo's 37.02 so not to far apart to worry about.