Sad to say I have somehow damaged my old Em3ev (cell man) triangle battery pack whilst in storage. This was always a brilliant pack, bought about 10 years ago, 16s5p (52v nominal using 3.3v LiFePo a123 26650 M1A cells. It was used lightly for about 5 years before I charged it and left it in storage, but at some point it has either fallen or else been crushed causing one cell to split open.
It's an old pack so I can't justify spending too much time or money, but it probably has a bit of life left as a spare battery. My thoughts are to either
1) cut out the 5th cell on each remaining parallel group you make them all 4p (to rectify the imbalance and just make it a smaller battery, or
2) solder in a replacement cell. It won't be a hard job to solder in, soldering obviously not best practice but I've successfully done it before, but I would need a recommendation for a replacement cell to use...bearing in mind these are 10 year old 2300mAh 3.3v M1A cells which would by now have lost appreciable capacity! I can get hold of the newer a123 26650M1B cells but these are 2500mAh.
Could I ask if anyone with experience building and repairing packs could give some advice?
TIA!!
It's an old pack so I can't justify spending too much time or money, but it probably has a bit of life left as a spare battery. My thoughts are to either
1) cut out the 5th cell on each remaining parallel group you make them all 4p (to rectify the imbalance and just make it a smaller battery, or
2) solder in a replacement cell. It won't be a hard job to solder in, soldering obviously not best practice but I've successfully done it before, but I would need a recommendation for a replacement cell to use...bearing in mind these are 10 year old 2300mAh 3.3v M1A cells which would by now have lost appreciable capacity! I can get hold of the newer a123 26650M1B cells but these are 2500mAh.
Could I ask if anyone with experience building and repairing packs could give some advice?